Greg Peterson
Structural
- May 10, 2021
- 5
I have been asked to look at a fix at a retail location involving corroded bottoms of tube columns. The tube is 8x8x3/16. The Contractor has welded a 3/8" plate all around it then at the top of the plates a 3/8" fillet weld to connect the plates to the TS. My concern with the 3/8" fillet weld is that it is too large for a 3/16" wall thickness. Too large meaning the weld went all the way through the TS wall and possibly created more problems than it solved.
The fix had already been implemented and I only had been asked as the Municipality wanted the approval of a structural engineer.
Any thoughts?
The fix had already been implemented and I only had been asked as the Municipality wanted the approval of a structural engineer.
Any thoughts?