Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Mechanical properties and allowable stresses

Status
Not open for further replies.

spike

Structural
Jun 7, 1999
46
Can anyone tell me the mechanical properties and allowable stresses for steel sheet/plate conforming to European grade P265GH?

Thanks
 
Replies continue below

Recommended for you

P265GH is a carbon steel material in accordance with EN 10028-2 (equivalent to A515 Gr.60)
Properties shown in this standard vary on plate thickness.
Which code are you going to use in the equipment design?
 
For plate thickness up to 16 mm and at room temp.
yield stress is 265 MPa and ultimate stress is between 410 and 530 MPa per En 10028-2.
Re allowable stress see previous answer
 
Status