Davkoo
Mechanical
- Jan 9, 2013
- 5
Hi,
I am trying to perform microhardness tests either in terms of Vickers or Knoop on Nylon 6,6 samples which have been weathered for quite a long time from 1 to 5 years.
The samples are cylindrical in shape with a diameter of 30mm and a length of 17mm but the most important thing to note is that surface cracks (max crack width measured was about 80 microns) were present mostly on the circular surface of the samples due to weathering.
Consequently, the problem I am having right now is that I cannot perform indentation directly on the circular surface because it is difficult to distinguish and hence to measure the indentations due to the presence of cracks.
Will I need to perform the tests rather on the cross-section of the samples or are there any other better alternatives? I am asking this because if I perform the tests on the cross-sections, I will need to machine the cross-sectional surfaces such that they are both flat and parallel to the bottom surface and I am not sure if machining the surface will affect the hardness measured.
Regards.
Regards
I am trying to perform microhardness tests either in terms of Vickers or Knoop on Nylon 6,6 samples which have been weathered for quite a long time from 1 to 5 years.
The samples are cylindrical in shape with a diameter of 30mm and a length of 17mm but the most important thing to note is that surface cracks (max crack width measured was about 80 microns) were present mostly on the circular surface of the samples due to weathering.
Consequently, the problem I am having right now is that I cannot perform indentation directly on the circular surface because it is difficult to distinguish and hence to measure the indentations due to the presence of cracks.
Will I need to perform the tests rather on the cross-section of the samples or are there any other better alternatives? I am asking this because if I perform the tests on the cross-sections, I will need to machine the cross-sectional surfaces such that they are both flat and parallel to the bottom surface and I am not sure if machining the surface will affect the hardness measured.
Regards.
Regards