kedminster
Electrical
- Nov 21, 2009
- 16
I am looking for test equipment to perform the Q (resonance) test outlined in MIL-46058C. This test is performed on coupon PCB's with a standard Y pattern an is used to evaluate the performance of coatings applied to the coupon.
Here is a link to the MIL spec I am referencing:
The test (section 3.11)requires that Q be measured at 1, 50 and 100MHz. Does anyone know anything further about ASTM D150 (I think this is the basis for this test) that may be relevant to test equipment selection?
Does anyone have a recommendation for an impedance analyzer for this application? Thanks in advance for any suggestion!
Karl Edminster
Does that smell like burning FR-4? Nah...just the FETs breaking in...
Here is a link to the MIL spec I am referencing:
The test (section 3.11)requires that Q be measured at 1, 50 and 100MHz. Does anyone know anything further about ASTM D150 (I think this is the basis for this test) that may be relevant to test equipment selection?
Does anyone have a recommendation for an impedance analyzer for this application? Thanks in advance for any suggestion!
Karl Edminster
Does that smell like burning FR-4? Nah...just the FETs breaking in...