The latest version of Subject standard defines two types of chemical: Type 1 and Type 2. These types determine if the chemical contains hexavalent chromium. The older version of the spec specified only classes of treatments: Class 1A and Class 3, for example, determine the thickness of the surface treatment.
What if one does not specify the Type of treatment and instead calls out only the Class of treatment? What Type of treatment is received by default? Or is the specification incomplete in that there is no default defined?