In my area (Northeast US) I do not typically see two way elevated slabs less than 8". Do others see/use less than this and if so what is a lower bound? I would think that 6" is pretty thin once tolerances and unknowns are accounted for, i.e. the 'd' being off by 1/2" in the field is a much larger percentage at 6" slab compared to 8". 7"?