Is there a guideline for the minimum distance between holes bored into a given thickness of aluminum plate?
We have a 1/16" thick plate that is ~7" diameter round of aluminum that requires 12 holes. It was suggested:
12X diameter 1.350"+- .005" thru, equally spaced at 30 degrees apart located on a diameter 5.400" BC.
So the hole centers are located radially from the center of the plate, but at these dimensions, the thickness between the holes is quite small. I want to stagger the holes, but was wondering if there is a rule for wall thickness between holes in this situation.
Thanks.
We have a 1/16" thick plate that is ~7" diameter round of aluminum that requires 12 holes. It was suggested:
12X diameter 1.350"+- .005" thru, equally spaced at 30 degrees apart located on a diameter 5.400" BC.
So the hole centers are located radially from the center of the plate, but at these dimensions, the thickness between the holes is quite small. I want to stagger the holes, but was wondering if there is a rule for wall thickness between holes in this situation.
Thanks.