Dear All,

We are procuring a valve. The material used is ASTM 182 F22. The material is having higher tensile strength , yield strength and hardness than normal F 22 materials. So is it acceptable?
And test certificate of this material will be certified as ASTM 182 F 22 ..will mention as modified . Is it acceptable

Regards,

Ratheesh N

 
Replies continue below

Recommended for you

There is no modified F22 in material specification ASTM A 182. You have Class 1 and Class 3 for F22 regarding strength and hardness. Regarding strength, there are no maximum requirements, only minimum requirements. The hardness for Class 1 is a maximum at 207 and for Class 3 is 156 to 207 Brinell.
 
"modified" in what sense? Do the chemical constituents meet ASTM A 182 spec? As it is forged, were the mechanical properties recorded after work hardening?

"...when logic, and proportion, have fallen, sloppy dead..." Grace Slick
 
If the mechanical properties and chemical requirements meet A-182 F22, it is stamped accordingly. If it does not meet all the requirements of the spec, it cannot be so stamped or stamped as F22 "modified".
 
Under the ASTM system you meet all of the spec requirements to certify the item, no exception only additions.
Does this spec have a max hardness, max strength, min elongation? Does the material meet these? If so then it meets the spec.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 