Need Help on Parameter setup for SS304 1/8'' and 1/4'' thick (Amada LC1212, Lens 5mm)........

Status
Not open for further replies.

Jackietran

Industrial
Apr 21, 2016
5
Hi all,

Could someone please post the cut conditions of parameter for SS304 1/8'' and 1/4'' Thick (Feed, Power, Freq, Focal, ect. ect.) I want to see where my conditions match with yours because i am getting a poor cut.

Thank you,
JT.
 
Replies continue below

Recommended for you

Firstly, are you using Nitrogen?
What are your current conditions?
 
C-SS0.134_plqgn3.jpg
C-SS0.250_kwrni5.jpg
 
hi evans1089,
we are using clean cut Nitrogen for stainless steel.
Thank you.
 
hi jjl1210,

Thank you for your reply but the power of our machine is 1500w, should I increase the duty to max.

Thank you,
JT
 
I would change all the 4000 to 1500 power and reduce the feed by 60% as a starting point. I started with a 2000w laser never 1500w but this is what I would try first.
 
Our 1500W for 1/4" was wide open and feedrate of 10 to 15. I would do a focus test and then try a different focus when cutting. Ours was -1.5 to -2.
 
Hi striker12300,

Thank you for your inform, i put my focal -.79 on lens 5mm but the burr is still at the bottom of sheet metal.
I will try different focal BTW can you post your Pierce & Edge setup screen for me.

Thank you,
JT.
 
Hi striker12300,

I will change the parameter setup and play around with it.

Thank you,
JT
 
Sorry I can't. It's no longer with us. Our setting were from an LCE655, but it was a 1500 watt laser.
 
I've also always found starting slow and working your way up to be the best bet. I run a 4kw Mazak U44-SG and overpowering the cuts seems to be quite common when I'm cutting anything that isn't => 3/8"
 