I have a BMW E36 with an LS2 V8 and T56 trans swapped in.
I am looking for input or correct formulas for calculating critical speed, spec out correct material dimensions/properties for my application.
Also I want to consider any other design factors that I may have overlooked.
I bought a kit for the swap that included an aluminum 3" diameter drive shaft. I've had this drive shaft repaired once and recently twisted the tube beyond repair.
Now I'm in need of a new drive shaft and plan to design it properly for my application.
The car makes 485rwhp/434rwtp. The current rear gear ratio is 3.23.
Drive shaft length is 43.5 inches U-joint center to center. Due to space constraints 3 inch diameter tube is max.
It's an IRS rear so the diff. is stationary.
The drive will run up to 7500 rpm when the car is on the race track. (possibly higher if I change to a shorter rear gear ratio)
The original DS that came with the swap kit has a
1350 U joint at the trans end and 1310/1350 conversion U joint at the diff end.
The configuration is like Style D in this link.
Any help with this would be greatly appreciated.
I am looking for input or correct formulas for calculating critical speed, spec out correct material dimensions/properties for my application.
Also I want to consider any other design factors that I may have overlooked.
I bought a kit for the swap that included an aluminum 3" diameter drive shaft. I've had this drive shaft repaired once and recently twisted the tube beyond repair.
Now I'm in need of a new drive shaft and plan to design it properly for my application.
The car makes 485rwhp/434rwtp. The current rear gear ratio is 3.23.
Drive shaft length is 43.5 inches U-joint center to center. Due to space constraints 3 inch diameter tube is max.
It's an IRS rear so the diff. is stationary.
The drive will run up to 7500 rpm when the car is on the race track. (possibly higher if I change to a shorter rear gear ratio)
The original DS that came with the swap kit has a
1350 U joint at the trans end and 1310/1350 conversion U joint at the diff end.
The configuration is like Style D in this link.
Any help with this would be greatly appreciated.