For the most part our reactors and tanks are 316L stainless. Most of the piping we have on site is 316 with some amount of 304 mixed in. We are wanting to work back through and identify what is 304 and what is 316.
Is there any easy means for testing where the piping and fittings are not clearly marked?
I have found a table of acid test on Engineering Tool Box
I additionally spoke to our local recycling center and they said they had a hand held alloy identifying analyzer made by Nycom?? I have not be able to find any information on such a tool.
Is there any easy means for testing where the piping and fittings are not clearly marked?
I have found a table of acid test on Engineering Tool Box