Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Nozzle loads on glass flake lined vessels

Status
Not open for further replies.

DSB123

Mechanical
May 16, 2002
1,288
Hi All,
Anyone out there know of any criteria for the limiting loads on vessel nozzles which have been glass flake lined? My feeling is the limiting criteria should be shell displacement and not stress limits using say WRC approaches or ASME VIII or EN13445. Any thoughts or advice of where this information is likely to be?
 
Replies continue below

Recommended for you

It may be an obvious question, but have you tried asking the manufacturer how they determine nozzle loads for such equipment?
 
The company I used to work for did a lot of glass-lined work. They would get allowable loads for equipment from the glass-lined equipment manufacturer.

When it came to glass-lined piping, they would run the simulation in Caesar. The failure criteria would be stress-based, but the allowable stress would be significantly reduced from the regular CS pipe. I can't remember the numbers for failure stress, but this may also have come from the glass lined pipe manufacturers.
 
XL83NL,marty007,
Ideal situation but the vessels are existing so not a valid way forward!!
 