EDub24
Structural
- Mar 8, 2016
- 185
I'm currently designing a partially buried reinforced fixed-base concrete tank. When determining the seismic loads I am using ACI 350.3-06 with the modifications per §15.7.7.3 of ASCE 7-16. That section of ASCE 7 requires you to replace the impulsive response modification factor of ACI 350.3, Ri, with the response modification factor, R, given in Table 15.4-2 of ASCE 7. In Table 4.1.1(b) of ACI 350.3 for a fixed base tank you are allowed to increase the response modification factor, Ri, from 2.0 for an at-grade tank to 3.0 for a buried tank with the ability to use linear interpolation if the tank is partially buried. It seems like ASCE 7 doesn't provide this option and only gives values for at-grade tanks. I'm interested in seeing what other people have done in this situation. Do you increase the response modification factor if the tank is partially buried or just stick with the factor given in ASCE 7?