Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PET Production via direct esterification of PTA

Status
Not open for further replies.

Ali G.

Chemical
Dec 30, 2021
3
Dear respectful elders of chemical/process engineering,

I'm working as a process engineer in place where produce virgin PET resin via direct esterification of PTA and MEG. Our MEG/PET ratio close to 335/1000 (kg/kg) and our managers push us to reduce this ratio.

Question is simple, what is your lowest EG/PET ratio in PET production? İs it possible to reach stoichiometric ratio? If answer is yes, how? Could you give some clue for your young colleague please :)

Best regards.

Ali
 
Replies continue below

Recommended for you

I'm not in this industry, but it seems to me that you aren't likely to get many answers in this regard.

Have you tried looking on Google or Google Scholar? Perhaps such knowledge is widespread and not secret. If so, you should be able to find literature on production processes and production ratios. If you can't find anything, it is likely that such process knowledge would be considered trade secret or a competitive advantage. As such, it would be unethical and unprofessional to share such knowledge.


 
Dear TiCl4,

You are definetely right but all threads in this forum also getting someone a competitive advantage, I think we should get over this to improve our industry.

İn addition, we love titanium too in our industry, thanks for your advice I ll dive into deep of google scholar:)
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor