Kindly give me your thoughts about issuing a piping certificate after inspection.
I have a client asking for a certificate after inspection of an in service piping.
The certificate shall contain parameters stating that the piping is fit for service for a certain duration.
Basically when I'm doing inspection as per API 570,the final documents I'm submitting after inspection is the final report
which contains my inspection findings,evaluation of NDE results and recommendations.
This certificate in my opinion is not a practical document to issue.
Any idea is appreciated,
Thanks and regards,
jb
Good day!
Kindly give me your thoughts about issuing a piping certificate after inspection.
I have a client asking for a certificate after inspection of an in service piping.
The certificate shall contain parameters stating that the piping is fit for service for a certain duration.
Basically when I'm doing inspection as per API 570,the final documents I'm submitting after inspection is the final report
which contains my inspection findings,evaluation of NDE results and recommendations.
This certificate in my opinion is not a practical document to issue.