What is the current thinking on using plastic bar chairs in a surface facing a high corrosion zone; b1 B1 or greater?
My understanding is that these can create a path that will enable the surrounding environment to permeate through the cover zone and so should not be used. (AS 3735—2001 - 4.4.4.4(c))
However this site shows that many engineers still recommend plastic chairs in these environments.
My understanding is that these can create a path that will enable the surrounding environment to permeate through the cover zone and so should not be used. (AS 3735—2001 - 4.4.4.4(c))
However this site shows that many engineers still recommend plastic chairs in these environments.