PLASTIC CAP CRAKING ON GLASS BOTTLES AFTER 7 TO 10 DAYS

Status
Not open for further replies.

T1G

Industrial
May 27, 2023
1
WE ARE FACING AN ISSUE OF CRACKING OF PLASTIC CAPS FITTED ON GLASS BOTTLES AFTER 7-10 DAS
 
Replies continue below

Recommended for you

Much more information required.
Cap screwed on too tight?