Hi
In a methanol plant, the bottom stream of Saturator equipment shows in its water analysis, the presence of chloride ion less than 1 ppm. Why is the chloride ion generated?

Result of sample parameters:
pH: 4.3
Conduct: 1520 uS/cm
TOC: 1100 ppm
Cl-: 0.3 ppm

NaOH its injected in the distillation unit and part of this remainder water (15 ton/h) its inlet stream of saturator equipment.

 
It is in one of your input streams. What is the flow in this bottom stream? It is likely that 99% of your Cl is ending up here, so in it's source material it may be 10ppt.
And why is the pH so low? Has this water been de-gassed?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 
No NaOH I've ever encountered was 100% free of Cl-, so that'd be the first place I'd look, unless I misunderstood your flowsheet.

Next guess is that it's an analytical artifact. What analytical method was used to detect 300 ppb of chloride reliably, and what is its detection limit?
 
What is the flow in this bottom stream?
R: 240 Ton/h
And why is the pH so low? Has this water been de-gassed?
R: The bottom stream it is recirculated to the Saturator. A part of this stream it is Blowdown. The pH is Low, because the stream it has not been de-gaseed yet.
Water entering the Saturator comes from two sources:
1) H2O remnant from distillation
2) H2O condensate of Reformed Gas.
I presume that the source of Cl- comes from the NaOH product that is injected to distillation and concentrates on the Saturator. Is it possible?
 
There is stainless steel piping. What temperature is dangerous for the material if I have a current with 1-10 ppm of Cl-?. Or it doesn't matter?
 
Which SS? There must be hundreds of grades of SS.

Good Luck,
Latexman
 
At this low of pH SCC is a real risk with 304.
What else in in this stream?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 
What is the flow in this bottom stream?
R: 240 Ton/h
And why is the pH so low? Has this water been de-gassed?
R: The bottom stream it is recirculated to the Saturator. A part of this stream it is Blowdown. The pH is Low, because the stream it has not been de-gaseed yet.
Water entering the Saturator comes from two sources:
1) H2O remnant from distillation
2) H2O condensate of Reformed Gas.
I presume that the source of Cl- comes from the NaOH product that is injected to distillation and concentrates on the Saturator. Is it possible?

RX Marine was established in 1996 in Mumbai, India; as chemical manufacturing company catering exclusively to the needs of the marine industry. In a short span of 12 years the company has established itself as one of the leading wholesale suppliers of a wide range of chemicals for - Marine industry internationally - and other local industires and plants. Our client list bears testimony to this. The RXSOL policy has its foundations on two pillars of strength - a continuous investment in research and development to deliver premium quality products and a commitment to service.

-------------------