8
Working on a battery with a steel casing.
Steel casing is lined with graphite paint but the zncl2 inside the battery still reacts with the steel.
Does Ag react with ZnCl2 ? is there a way to coat Pure graphite on steel (enough to prevent the reaction with ZnCl2)
I have tried to use 0.02mm pure graphite flake foil whoch seems to work but will be cost prohibitive in mass production.

Thanks
 
Replies continue below

Recommended for you

An epoxy paint should work. Steel and graphite in a ZnCl2 electrolyte makes for a very good battery in itself and corrosion rate will be very high.
 