I have a Prima Domino Laser cutter that was just purchased a year ago (used) to cut mild steel tubes with no problem. Now trying to cut .0625 (16ga) SS with not so great success, my issue is its creating a ton of dross on the bottom of the cut.
When I reference documents from Trumpf for SS the parameters seem totally different. Could anyone advise? Thanks.
Nozzle - 2.0mm Single Nozzle
Here are my cutting parameters.
Feed (80in/min)
Power (3500W)
Freq. (0)
Duty (0)
Gas (11Bar)
Stand Off (.04mm)
Focus(-.1in)
Piercing
Power (2800W)
Freq. (190Hz)
Duty (60%)
Gas (2bar)
Stand Off (.150mm)
Focus (-.040in)
When I reference documents from Trumpf for SS the parameters seem totally different. Could anyone advise? Thanks.
Nozzle - 2.0mm Single Nozzle
Here are my cutting parameters.
Feed (80in/min)
Power (3500W)
Freq. (0)
Duty (0)
Gas (11Bar)
Stand Off (.04mm)
Focus(-.1in)
Piercing
Power (2800W)
Freq. (190Hz)
Duty (60%)
Gas (2bar)
Stand Off (.150mm)
Focus (-.040in)