KMP04
Mechanical
- Mar 23, 2004
- 22
PROBLEM: Unfortunately site has no more 1.5" square PTFE braided packing in stores for their water seal stuffing box, located on one of their hydraulic turbine units.
Shipping is 7-10 days and they need the unit online ASAP. The question is, can we compress 1.25" square braid (in stock) to fit into the 1.5" gap to form a sufficient water seal until the right packing arives on site?
The turbine shaft is 16" dia., rotates at 150rpm & the river water temp would not exceed room temperature. Maximum pressure is aprox. 30psi. My only concern was if the 1.25" packing was not compressed enough, it could loosen and uncoil or simply allow excessive leakage.
Anyone have experience with this kind of application?
Thanks, KMP
Shipping is 7-10 days and they need the unit online ASAP. The question is, can we compress 1.25" square braid (in stock) to fit into the 1.5" gap to form a sufficient water seal until the right packing arives on site?
The turbine shaft is 16" dia., rotates at 150rpm & the river water temp would not exceed room temperature. Maximum pressure is aprox. 30psi. My only concern was if the 1.25" packing was not compressed enough, it could loosen and uncoil or simply allow excessive leakage.
Anyone have experience with this kind of application?
Thanks, KMP