Dec 16, 2008 #1 Xeros Materials Dec 5, 2006 54 0 0 KR Hi, i'm Xeros In accordance with API610, CI or CS could be used for the casing material. I have question between CI and CS. Sometimes, CI is used for casing material, sometimes CS. Could i know the detailed reason why sometimes, CI is selected or sometimes CS?
Hi, i'm Xeros In accordance with API610, CI or CS could be used for the casing material. I have question between CI and CS. Sometimes, CI is used for casing material, sometimes CS. Could i know the detailed reason why sometimes, CI is selected or sometimes CS?
Dec 16, 2008 #2 nickelkid Mechanical Jan 8, 2003 422 0 0 US What is your application? Upvote 0 Downvote
Dec 16, 2008 Thread starter #3 Xeros Materials Dec 5, 2006 54 0 0 KR Sorry, Generally fire water pump or liquid sulfur service Upvote 0 Downvote
Dec 16, 2008 #4 Artisi Mechanical Jun 11, 2003 6,458 0 36 AU CI for fire service cs (cast steel) for liquid sulphur. Upvote 0 Downvote
Dec 16, 2008 Thread starter #5 Xeros Materials Dec 5, 2006 54 0 0 KR Thank you for your help. AND MORE, I want to know the reason CI for Fire Service and CS for Liquid Sulfur. Is the reason that CS is more corrosion resistant than CI? Or mechanical properties? Upvote 0 Downvote
Thank you for your help. AND MORE, I want to know the reason CI for Fire Service and CS for Liquid Sulfur. Is the reason that CS is more corrosion resistant than CI? Or mechanical properties?
Dec 16, 2008 #6 Artisi Mechanical Jun 11, 2003 6,458 0 36 AU CI is sufficient for the fire service whereas CS in a better choice as it's much safer for pumping hot liquid sulphur - not subject to failure from thermal shock which CI is. Upvote 0 Downvote
CI is sufficient for the fire service whereas CS in a better choice as it's much safer for pumping hot liquid sulphur - not subject to failure from thermal shock which CI is.