Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PVC fabric span

Status
Not open for further replies.

bradatocudoviste

Civil/Environmental
Oct 29, 2012
3
Im trying to validate a PVC fabric as a cladding supported by steel frames. My frames have a 20m (66ft) span and a bay spacing of 4m (13ft).
LL is 1,25kN/m2 (26psf) - snow (dominant)

What I have from PVC membrane manufacturer site is
tensile strength 250/250 daN/5cm (285 lb/in)
tear strength 20/20 daN/5cm (22 lb/in)

Where can i find some guides/codes for a simple calc on this subject?

ty
 
Replies continue below

Recommended for you

Treat the fabric as a 12-inch wide strip of catenary with your loads applied uniformly. 285 lbf/in is a reasonably robust fabric. You can also model as a membrane in FEA.
 