Table 311.1.3 states P1 material a preheat of 200°F for thickness of >1". The table name is Exemptions to Mandatory Postweld Heat Treatment.
Does that mean I must:
1. Preheat to 200°F if my material is over 1"?
or
2. Preheat to 10°C for example then PWHT if my material is over 1"?
Or is it only PWHT over 1" if required as per job and then I have an option to PWHT or Preheat to 200°F
Seems somewhat missleading.
Does that mean I must:
1. Preheat to 200°F if my material is over 1"?
or
2. Preheat to 10°C for example then PWHT if my material is over 1"?
Or is it only PWHT over 1" if required as per job and then I have an option to PWHT or Preheat to 200°F
Seems somewhat missleading.