Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ready mix design

Status
Not open for further replies.

nada2013

Civil/Environmental
Jan 17, 2013
8
Hi everyone.
Can you give me an approximated ready mix design for compressive strength of 30Mpa and maximum size of aggregate 10 mm and the finess modulus of fine aggregate 2.8?





 
Replies continue below

Recommended for you

Check with a possible/likely concrete supplier to the project for some examples. They have been through this many times before and probably have a library of mix designs and test reports from previous projects.

Since concrete is over 80% local aggregates, a mix from elsewhere will mean nothing for your specific project. Maximum aggregate size is usually fine if the materials are crushed. For fine aggregates, an fm may not be indicative because particle shape has a high effect on placement and finishing. If you have a large project (over 1000 cubic yards), specific aggregates may be trucked in at high eventual cost since the specific mix will be shopped out and require additional testing and time.

Why do want to design a mix and not make appropriate performance requirements (compressive strength, w/c ratio, slump and placement/curing)?

Dick

Engineer and international traveler interested in construction techniques, problems and proper design.
 
nada2013...agree with CM. Also, it is against forum rules to post the same question in multiple forums. Please delete your other post.
 
ok, I think I make a mistake> i will delete it . thank you.
 