relationship between hardness and Young's modulus in polymers

Status
Not open for further replies.

agb253

Mechanical
Jul 28, 2010
4
Is there a reliable equation relating hardness to Young's modulus for polymers? I have a piece of polymer that would be hard for me to machine into a good tensile testing sample but it might be easy to perform a hardness test.

Please help.
 
Replies continue below

Recommended for you

I guess if that worked then everyone would be doing it. Sounds interesting, though.
 
No.
Hardness is mostly driven by strength, though in low modulus materials there is a stiffness component.
If you are working with a type of hardness measurement that is in the fully elastic range then you might be able to develop one.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
agb...I can't imagine such a correlation being very accurate if one exists at all.

Have you considered freezing the polymer before/during machining?

 