hi all!
we are facing a huge problem. We have mc quary make water based chiller system for cooling our control room and other halls. the problem is that we have refubrished the whole system. Only condersnors ( forced air - cooled) and frame left original. All other we install by our own. We have installed six copeland 7.5hp sealed screw compressors (original design was also of six compressors). and we installed all other accessories necessary and we got our system installed with some people having great expreince in chiller systems and they professionally do this business. But after 15 days of extremely successfull operation (when it goes on the temperature inside falls from 30 deg C to 7 deg C), suddenly compressors started burning. and we started to replace burned compressors with some refubrished (piston type compressors due to limitation of budget). We also hired some other professionals and they also tried but the problem is persistent.
Both are unable to give us any solid reason or able to fix the problem. Compressors are continously still getting their winding short (even refubrished piston).
We are using honeywell r-22 original usa made refigerant gas and silo compressor oil made for low temperatures.
Kindly help us.
Thanks in advance.
we are facing a huge problem. We have mc quary make water based chiller system for cooling our control room and other halls. the problem is that we have refubrished the whole system. Only condersnors ( forced air - cooled) and frame left original. All other we install by our own. We have installed six copeland 7.5hp sealed screw compressors (original design was also of six compressors). and we installed all other accessories necessary and we got our system installed with some people having great expreince in chiller systems and they professionally do this business. But after 15 days of extremely successfull operation (when it goes on the temperature inside falls from 30 deg C to 7 deg C), suddenly compressors started burning. and we started to replace burned compressors with some refubrished (piston type compressors due to limitation of budget). We also hired some other professionals and they also tried but the problem is persistent.
Both are unable to give us any solid reason or able to fix the problem. Compressors are continously still getting their winding short (even refubrished piston).
We are using honeywell r-22 original usa made refigerant gas and silo compressor oil made for low temperatures.
Kindly help us.
Thanks in advance.