YuJie_PV
Mechanical
- Jan 19, 2017
- 135
hi all,
we have flanged joint with ring type joint. flange is 304, ring type joint 304 too. we mandate that the hardness of flange shall be larger than that of ring type joint by min.30HB.
now the materials are purchased already, and test result is beyond original expectation:
the hardness of ring type joint (304) is 147HB;
the hardness of flange material 304(raw material, not fabricated into finished product yet) is 158HB.
is there any method which may help achieve a wider hardness difference between ring type joint gasket and flange?
thanks in advance.
we have flanged joint with ring type joint. flange is 304, ring type joint 304 too. we mandate that the hardness of flange shall be larger than that of ring type joint by min.30HB.
now the materials are purchased already, and test result is beyond original expectation:
the hardness of ring type joint (304) is 147HB;
the hardness of flange material 304(raw material, not fabricated into finished product yet) is 158HB.
is there any method which may help achieve a wider hardness difference between ring type joint gasket and flange?
thanks in advance.