48
One of our customers has asked us to fabricate a replacement air receiver tank for their facility. The existing vessel is designed for 125psi @ 650deg. F and is constructed of SA-455 material. I would propose using SA-516-70 for the construction of the replacement vessel due to availability. I've checked the stress values allowed for each material in Section II Part D - they are the same at 650deg. F.

What, if any advantages are there to using SA-455 material as opposed to SA-516-70?

Any input would be appreciated.
 
Replies continue below

Recommended for you

Go with the SA 516 Gr 70. Improved notch toughness.
 
SA455 Heads should be available commercially they are std parts, shell is different.
 