hi everybody
in our assemble line we have a problem. we use a M6 screw with a grade of T7. the screw must pass 3 steel sheets.unfortunately the holes in these 3 sheets are not concentric and that causes the screw to get striped or fractured while fastening with screwdriver. for the time being it is impossible for us to modify the sheet molds and the place of holes. is there any way that with changing the design or heat treatment of screw i can prevent stripping?
best regards
in our assemble line we have a problem. we use a M6 screw with a grade of T7. the screw must pass 3 steel sheets.unfortunately the holes in these 3 sheets are not concentric and that causes the screw to get striped or fractured while fastening with screwdriver. for the time being it is impossible for us to modify the sheet molds and the place of holes. is there any way that with changing the design or heat treatment of screw i can prevent stripping?
best regards