Good morning everybody
J'm interested in selection of material for seals which will control air flow to a diesel engine.
Temeperature range of the gasket: Temperature range = -40 ºC to +170 ºC
Maximum internal pressure (Pi) = 3.2 bar absolute.
Pressure range across the seal = -0.275 bar to +2.2 bar relative.
Fluid resistance
The seal shall be able to resist the following:-
Diesel fuel.
Bio diesel.
Engine oil.
Engine coolant / ethylene glycol
J am thinking about rubber based on FKM material.
Could anybody help me with selectiong approporiate material for this purpose?.
Thank You
Mike
J'm interested in selection of material for seals which will control air flow to a diesel engine.
Temeperature range of the gasket: Temperature range = -40 ºC to +170 ºC
Maximum internal pressure (Pi) = 3.2 bar absolute.
Pressure range across the seal = -0.275 bar to +2.2 bar relative.
Fluid resistance
The seal shall be able to resist the following:-
Diesel fuel.
Bio diesel.
Engine oil.
Engine coolant / ethylene glycol
J am thinking about rubber based on FKM material.
Could anybody help me with selectiong approporiate material for this purpose?.
Thank You
Mike