Hi everyone,
We are using a horizontal rotating vessel/mixer made of SA-283 Grade C. Due to erosion the vessel shell needs to be replaced every two three years. How do I select a better material with higher hardness, economical and that can easily fabricated. Any standard for selection of vessel material. The medium temperature is approximately 100C and pressure is atmospheric.
We are using a horizontal rotating vessel/mixer made of SA-283 Grade C. Due to erosion the vessel shell needs to be replaced every two three years. How do I select a better material with higher hardness, economical and that can easily fabricated. Any standard for selection of vessel material. The medium temperature is approximately 100C and pressure is atmospheric.