Guys,
Anyone face this issue before? the parts do tend to be on the blackish side after shot blasting - shots used s110, material shot blasted = hot rolled/ cold rolled steel cages....this especially is an issue when new shots are added...
need to run "dummy lots" with scrap parts to lighten the shade...after a couple of hrs run the shots do indeed give lighter shade shot blasted parts...
very weird? anyone think media work-balance issue? anyway to resolve this...we do regular sieve analysis and they do pass...
any help appreciated
Anyone face this issue before? the parts do tend to be on the blackish side after shot blasting - shots used s110, material shot blasted = hot rolled/ cold rolled steel cages....this especially is an issue when new shots are added...
need to run "dummy lots" with scrap parts to lighten the shade...after a couple of hrs run the shots do indeed give lighter shade shot blasted parts...
very weird? anyone think media work-balance issue? anyway to resolve this...we do regular sieve analysis and they do pass...
any help appreciated