Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Slip On Flanges

Status
Not open for further replies.

BJaffa

Industrial
Nov 5, 2002
27
Why does the B31.1 limit S/O flanges to NPS 4 and Class 300 per Par(s) 104.5.1(A), 122.1.1 (F) and Fig 127.4.4(B)? Can or should one design around this restriction?
 
Replies continue below

Recommended for you

The main reason should be the lower fatigue resistance of those flanges with respect to weld neck.
If you are bound to B31.1 as the code, I can't see how you could circumvent that rule: you should switch, if you can, to a less demanding code, such as B31.3.