I noticed that MasterSpec doesn't allow a spray cure compound for floor slabs to receive a floor covering, i.e. a form of wet cure is required. I know that dissipating spray curing compounds sometimes do not dissipate if they are not exposed to light and foot traffic, but they still seem to be the most common method of curing. Am I wrong about that? I would like to hear what you guys are specifying.