Spring material Inconel

Status
Not open for further replies.

Isha90

Mechanical
Dec 21, 2017
88
Inconel X750 & X650, Which is the best out of two material for Spring used in Lift Check Valve, please
 
Replies continue below

Recommended for you

1. Which can you get?
2. Does corrosion resistance matter?
3. which is stronger?
What does the supplier suggest?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Valves are used in both Power & Process industry, High temperature & Corrosion application please
 
I think Inconel 750 is for more common. Very hard to give specific recommendation when no specific information is given. What constitutes "best" to you?

----------------------------------------

The Help for this program was created in Windows Help format, which depends on a feature that isn't included in this version of Windows.
 
Isha...

LOTS of data for X-750 [UNS N07750], which is generally recommended for aerospace applications... including springs
Go to ... click on 'Inconel Alloys' tab... download data for X-750 TDS.

MatWeb Inconel Data sheets do NOT include X-650
INCONEL® Technical Data Sheets

Can't say anything about X-650... I cannot recall even hearing about it! I looked in my Metallic Materials Specification Handbook [4ed] and came-up 'dry'.

EdStainless: You have a clue-card where to find X-650 data?

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
To be honest the only X-650 data that I have is not for spring temper material.
As far as I know X650 is not an industrially significant alloy.
It would be common today to use alloys such as A286, 718, or even cold worked 600 or 625.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 