amsomu04
Mechanical
- Jan 20, 2009
- 19
Hello all,
Recently we sent the dish blank for forming operation. While forming the dish end, the base material was broken up to 1 feet from 4 inch away from the weld joint. The condition of received plate was HOT ROLLED, ANNEALED AND PICKLED. Plate Thk.10mm. Welding consumable used E309/E309L. No pre heat given since the PQR passed without preheat.
Request all to give your feedback of what could be the reason for this failure.
Thank you..
Recently we sent the dish blank for forming operation. While forming the dish end, the base material was broken up to 1 feet from 4 inch away from the weld joint. The condition of received plate was HOT ROLLED, ANNEALED AND PICKLED. Plate Thk.10mm. Welding consumable used E309/E309L. No pre heat given since the PQR passed without preheat.
Request all to give your feedback of what could be the reason for this failure.
Thank you..