Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stainless steel, chlorine dioxide & low pH

Status
Not open for further replies.

dunn782

Mechanical
Apr 9, 2003
4
I have an application for a livestock water systems that has several water treatments added. One of the additives is anthium dioxcide and the other is sodium bisulfate. The sodium bisulfate is a dry acid added to lower the pH to 3-4 range for a variety of reasons. The anthium dioxcide will form chlorine dioxide in the system and is used for sanitation. The problem is there are components in the system that are 300 series SS and there are signs of pitting and/or discoloration. The sodium bisulfate at that level alone doesn't seem to create the same problem with a lab test. Could the chlorine dioxide present in the low pH be creating the problem? This occurs in only a few day exposure.
 
Replies continue below

Recommended for you

Just about guaranteed to do the job. You have all the ingredients to do a number on 304 SS.

Can you comeback with some levels of the chloride and sulfate ions? There are several questions and this might help to better understand your problem and recommend a possible solution.
 