Hi,
I am new to this forum and i am no expert.
So, in short, mechanical department asked me to buy anchor bolt for their equipment. It is decided to use SUS 316 anchor bolt. I refer to ASTM A193 B8M class 1 with ASTM A194 grade 8M (heavy hex) for nut. For washers, i am not sure as to what specification should i use.
If refer to ASTM F436 (hardened flat washer), it seems that it does not apply for SUS 316.
What specification of washer that apply with SUS 316? And should i use round hardened flat washer or square plate / plate washer? For information, the hole size of my base plate is 40mm and anchor size would be M30 (30mm). We use metric here in Indonesia.
Thanks for your kind attention.
Regards,
I am new to this forum and i am no expert.
So, in short, mechanical department asked me to buy anchor bolt for their equipment. It is decided to use SUS 316 anchor bolt. I refer to ASTM A193 B8M class 1 with ASTM A194 grade 8M (heavy hex) for nut. For washers, i am not sure as to what specification should i use.
If refer to ASTM F436 (hardened flat washer), it seems that it does not apply for SUS 316.
What specification of washer that apply with SUS 316? And should i use round hardened flat washer or square plate / plate washer? For information, the hole size of my base plate is 40mm and anchor size would be M30 (30mm). We use metric here in Indonesia.
Thanks for your kind attention.
Regards,