Feb 9, 2004 #1 dulmant Mechanical Jan 31, 2003 9 0 0 PT Hi, Does anybody knows what are the ultimate and the yield strength values for Steel DIN CK75 (and CK67), used for DIN 2093 disc washers? Thank you, dulmant
Hi, Does anybody knows what are the ultimate and the yield strength values for Steel DIN CK75 (and CK67), used for DIN 2093 disc washers? Thank you, dulmant
Feb 9, 2004 1 #2 ijzer Materials Oct 25, 2002 313 0 0 NL German material CK75 : Y = 1275 N/mm2 minimum, Tensile 1320-1870 N/mm2 Upvote 0 Downvote
Feb 9, 2004 Thread starter #3 dulmant Mechanical Jan 31, 2003 9 0 0 PT Thanks ijzer, Where did you get this? Any refference? dulmant Upvote 0 Downvote
Feb 10, 2004 #4 ijzer Materials Oct 25, 2002 313 0 0 NL See the "Stahlschluessel CD" go to CK75 and ask for properties. For info on this CD see http://www.stahlschluessel.de Upvote 0 Downvote
See the "Stahlschluessel CD" go to CK75 and ask for properties. For info on this CD see http://www.stahlschluessel.de
Feb 10, 2004 Thread starter #5 dulmant Mechanical Jan 31, 2003 9 0 0 PT Thank you very much. dulmant Upvote 0 Downvote