Need your opinion. I am no welding expert.
I am trying to weld a small shield plate (3mm) (non-structural) to a frame.
However, I am concern with the potential warping of the thin plate.
Thinking of doing stitch welding to mitigate this (as opposed to full perimeter weld), but I am concern with it susceptibility to corrosion, and as well as poor fusion.
And stitch welding itself could potentially does not mitigate warping due to localize heating.