azmirosman
Mechanical
- Jan 11, 2019
- 20
Dear All,
Good Day.
I need your guidance on the require testing and precaution when dealing with clad material normalizing.
Basically i'm dealing with one project which the head of the vessel need normalizing due to fiber elongation exceed the acceptable limit.
I'm requesting from contractor and vendor on the heat treatment procedure and the procedure was prepared as per clad plate mill certificate temperature and cooling rate.
My question:
Is there any guideline or precaution or any testing require after the heat treatment to check the condition of the bonding or clad material itself.
Edit:
Base Metal is Sa 516 Gr.70 (30mm) with SS316L clad.Fiber elongation calculated is 7%.
I don't have any experience on this.
Appreciate your response
Good Day.
I need your guidance on the require testing and precaution when dealing with clad material normalizing.
Basically i'm dealing with one project which the head of the vessel need normalizing due to fiber elongation exceed the acceptable limit.
I'm requesting from contractor and vendor on the heat treatment procedure and the procedure was prepared as per clad plate mill certificate temperature and cooling rate.
My question:
Is there any guideline or precaution or any testing require after the heat treatment to check the condition of the bonding or clad material itself.
Edit:
Base Metal is Sa 516 Gr.70 (30mm) with SS316L clad.Fiber elongation calculated is 7%.
I don't have any experience on this.
Appreciate your response