NDTHAND1992
Mechanical
- Apr 9, 2014
- 14
I have a customer that wants to know if he can stub in a 6" branch pipe to a 16" run pipe both sch.40 P1 material utilizing his existing groove weld procedure or does a branch connection need a completely new procedure and welder qualification. My first answer was yes that is permissible since the procedure lets them complete unlimited fillets and the groove welds up to .864". I do not have access to section IX at this time. Thoughts please ?