Dear All
I have two question regarding material selection for Stud Bolt.
1. Can i select B7 alloy steel stud bolts for SS 316 or SS304 flanges , if it is acceptable how can i justify galvanic corrosion issue due to dissimilar metal contact issue. Any standard reference is highly appreciated. Line class 150, Design Pressure 10 Bar. Design temp 122 F, Service water.
2. Is there any reference or standard to stud selection as per environmental condition, means stud or bolt shall be galvanized or non galvanized or any type of coating is applicable.
3. if all stud are non coated and later on we observed corrosion on studs can we apply the paints or cold galvanizing on all stud without removing from the flange joints.
Please send me any standard reference.
Regards
I have two question regarding material selection for Stud Bolt.
1. Can i select B7 alloy steel stud bolts for SS 316 or SS304 flanges , if it is acceptable how can i justify galvanic corrosion issue due to dissimilar metal contact issue. Any standard reference is highly appreciated. Line class 150, Design Pressure 10 Bar. Design temp 122 F, Service water.
2. Is there any reference or standard to stud selection as per environmental condition, means stud or bolt shall be galvanized or non galvanized or any type of coating is applicable.
3. if all stud are non coated and later on we observed corrosion on studs can we apply the paints or cold galvanizing on all stud without removing from the flange joints.
Please send me any standard reference.
Regards