Dear All,
I'm looking for an alternative to using Type V cement on a project. The soluble sulphates are as high as 1.9% and chlorides vary between 8-22%.
I've looked at various waterproofing additives but they tend to make very generalized statements about "improved chemical resistance".
Another option is the use of Silica Fume but again from my research I am only able to get general comments.
Has anyone had any success using an alternative and or details for using silica fume?
Thanks
I'm looking for an alternative to using Type V cement on a project. The soluble sulphates are as high as 1.9% and chlorides vary between 8-22%.
I've looked at various waterproofing additives but they tend to make very generalized statements about "improved chemical resistance".
Another option is the use of Silica Fume but again from my research I am only able to get general comments.
Has anyone had any success using an alternative and or details for using silica fume?