mecoman
Mechanical
- Dec 11, 2006
- 36
Hi All,
Looking for sources to supply AllOY 2507, 904L or similar specs. Trouble we are having is stock size. We need at least 3" thick plate, 4" would even be better. Approx plate OD is 24".
We are only able to source 1.5" thick plate.
Application has exposure to the following chemistry:
55% concentrated acetic acid
30% concentrated formic acid
15% h2o
all at 105C
Any insight is appreciated. Alternative material suggestions welcome.
Enjoy the day and remember, today is a good day to live.
Cheers,
MECOMAN
Looking for sources to supply AllOY 2507, 904L or similar specs. Trouble we are having is stock size. We need at least 3" thick plate, 4" would even be better. Approx plate OD is 24".
We are only able to source 1.5" thick plate.
Application has exposure to the following chemistry:
55% concentrated acetic acid
30% concentrated formic acid
15% h2o
all at 105C
Any insight is appreciated. Alternative material suggestions welcome.
Enjoy the day and remember, today is a good day to live.
Cheers,
MECOMAN