thread292-381691

I could not find the table 331.1.1 which says about the PWHT thickness in my CASTI Guidebook to ASME B31.3, please help

 
Replies continue below

Recommended for you

Table 331.1.1 is on page 73 of the 2016 edition of B31.3.
 