We need to coat the stainless steel springs with teflon (25-30 microns)in order to increase the corrosion resistance. The spring wire diamter is 0.55mm and its un-compressed length is 9.5mm. We tried a few times but failed to achieve the continuous teflon coating all round the spring wire. The suppliers say that the coating process is difficult since the item is too small.
Could any one guide us on this please.
Thanks
We need to coat the stainless steel springs with teflon (25-30 microns)in order to increase the corrosion resistance. The spring wire diamter is 0.55mm and its un-compressed length is 9.5mm. We tried a few times but failed to achieve the continuous teflon coating all round the spring wire. The suppliers say that the coating process is difficult since the item is too small.