itez
Structural
- May 5, 2013
- 52
Can you see anything wrong with chipping the edge of slabs to enable hands to enter it and for carbon fiber to be wrapped around beams and then epoxy back (epoxy grout) the slabs avoiding cutting any rebars? Would this be as strong as original slab? Why and why not?