I am working on a problem involving spray dryers. The material to be dryed would be injected through a rotating nozzle with multiple openings from the top. Hot air would be blown from the dryer's bottom part. I was wondering how can I approach the problem to find out the particle's terminal velocity and how is terminal velocity related to reynolds number.any help will be appreciated.

thanks

 
Replies continue below

Recommended for you

There are many empirical relations describing incipient fluidization velocity or minimum fluidization velocity or critical Re.You can find them in numerous books and papers. The equations will give you a range of values that may differ quite a lot.Here I've got some of them from one of my spread sheets

fuidization Re:
*Vane?ek,*Pavlov
Re=Ar/ [1400 +5,22*sqrt(Ar)]
*Rhodes (eq. 8) from:
Ar=1406 *Remf+27,3 * Remf**2
Geldart (p24 eq. 2.26) from:
Ar=1650*Remf+24,5*Remf**2
*Wen & Yu from:
Ar=1652*Remf+24,5*Remf**2

minimum fluidization velocity
*Rhodes (eq.10)
Re_mf=33,7*[SQRT(1+3,59e-5*Ar) -1]
Rhodes (eq. 7)
Re_mf =[-150*(1-epsilon)+-sqrt((150*(1-epsilon))**2+4*1,75*epsilon**3*AR)]/( 2*1,75)

*Kneule p.320
Re L =[1830 + 0,571*epsilon_L**3*Ar/(1-epsilon_L)**2]**1/2 - 42,8
*Kneule p.320
u_mf=Re_L*(1 - epsilon)*viscosity/d_p
Geldart (p24 eq. 2.27)
u_mf=m / (ro_fl*d_p) * [sqrt(1135,7+0,0408*Ar)-33,7]
Bulk Solids Physical Properties Guide
u_mf=420*ro_p*d_p**2

incipient fludization velocity
*Rhodes from:
Ar=150*(1-epsilon)*epsilon**3*Re_mf+1,75/e**3*Re_mf
*Rhodes from:
Re_mf=33,7*[SQRT(1+3,59e-5*Ar) -1] ---->u_mf

*Pavlov p.123:
v_cr=Re_cr*viscosity_fl/d_p

Re.. Reynolds number
Ar-Arhimedes number
epsilon -porosity
e_L- porosity
u_mf-minimum fluidization velocity
ro-density
viscosity
d_p- particle diameter
ro_fl-fluid density
v -velocity
index fl--fluid
index cr-critical
index mf-minimum fluidization

If you need citated papers it will take me some time to find them.